SEARCH FINESCALE.COM

Enter keywords or a search phrase below:

Surface preparation question

1935 views
7 replies
1 rating 2 rating 3 rating 4 rating 5 rating
  • Member since
    September 2016
Surface preparation question
Posted by twodollarcoin on Saturday, September 10, 2016 11:07 AM

G'day Modellers,

Only just recently got back into scale modelling since I was a teenager. This forum and google have been a great help, but I am in need of some information.

I've got a Ta-152 on the bench, painted and gloss-coated with future. My concern is that either (a) The Tamiya acrylic paint dried too quickly leaving the surface too rough or (b) I've airbrushed the future incorrectly.

Please see the attached photo, I think the surface is still too rough to apply the decals?

Any advice would be appreciated :)

Thanks,

Chris

 

  • Member since
    November 2009
  • From: Twin Cities of Minnesota
Posted by Don Stauffer on Tuesday, September 13, 2016 8:45 AM

Don't see any photo.

Don Stauffer in Minnesota

  • Member since
    January 2013
Posted by BlackSheepTwoOneFour on Tuesday, September 13, 2016 9:23 AM

Don Stauffer

Don't see any photo.

 

 

Me neither....

  • Member since
    January 2014
  • From: Nampa, Idaho
Posted by jelliott523 on Tuesday, September 13, 2016 9:59 AM

Ditto

If I had to guess, since there is no picture, I'd assume that 1) the paint, did exactly as you stated, and dried somewhat before it hit the surface creating a rough, pebbley texture or 2) the gloss coat did the same thing, or 3) the surface of the plastic was not properly prepared for painting and there are dust, hair or other foreign materials on the plastic. One thing I always try to do before I apply a gloss coat is to check the paint surface first, if it feels rough, then I will use a fine sanding pad or sanding stick and smooth out the paint, at this point it is possible that I need to apply another light coat of paint. Proper surface prep of the bare plastic is essential as well. I like to wipe the plastic down with a soft, lint-free cloth dampened with 91% isopropyl alcohol.

On the Bench:  Lots of unfinished projects!  Smile

  • Member since
    September 2016
Posted by twodollarcoin on Tuesday, September 13, 2016 2:44 PM

Sorry Guys, link didn't work. Here it is:

 

Wing Surface

 

 

 

  • Member since
    November 2009
  • From: Twin Cities of Minnesota
Posted by Don Stauffer on Wednesday, September 14, 2016 9:37 AM

In some cases like that I have salvaged the situation by sanding the areas that need decals with #600 wet or dry sandpaper, used wet, then re-applied the gloss coat.  After decaling, the dullcoat should make all areas pretty much the same flatness.

 

Don Stauffer in Minnesota

  • Member since
    September 2016
Posted by twodollarcoin on Sunday, October 16, 2016 11:51 AM

Hi Don,

 

After a small break I followed your advice and the decals have come up well! I've never used the Microsol Set/Sol combination before, it has great results... the decals actually sink into the panel lines. Very nice!

  • Member since
    November 2008
  • From: Central Florida
Posted by plasticjunkie on Wednesday, October 19, 2016 10:23 PM

I usually take an old soft cotton t shirt and polish out the surface after the paint dries. If still rough then I use a super fine pad 800 or above to lightly smooth things out then the gloss goes on.

I like using Solvaset over Micro set and sol because I find it to work much better.

 

 GIFMaker.org_jy_Ayj_O

 

 

Too many models to build, not enough time in a lifetime!!

JOIN OUR COMMUNITY!

Our community is FREE to join. To participate you must either login or register for an account.

SEARCH FORUMS
FREE NEWSLETTER
By signing up you may also receive reader surveys and occasional special offers. We do not sell, rent or trade our email lists. View our Privacy Policy.