Alclad II skinning over in airbrush

1037 views
0 replies
1 rating 2 rating 3 rating 4 rating 5 rating
  • Member since
    May 2006
  • From: Chapin, South Carolina
Alclad II skinning over in airbrush
Posted by Shipwreck on Wednesday, September 14, 2016 10:47 AM

 

 

 

Alclad II skinning over in airbrush

 

 

I am having a problem with Alclad II, ALC 106, White Aluminum. It is forming a skin in my airbrush. The skin breaks into chips that are clogging the nozzle at 15 to 20 psi. The chips are thin enough that I can blow them out by opening the airbrush while spraying into a jar; but clogs right up again when I go back to the model. I have not had a problem with any other colors. Is anyone else experiencing this with White Aluminum?

 

Thank you for any suggestions!

On the Bench:

Revell 1/96 USS Constitution - rigging

Kinetic 1/48 YF-104A 5-2957

Trumpeter 1/350 USS Hornet CV-8

Revell 1/48 B-1B Lancer Prep & Reasearch

 

 

JOIN OUR COMMUNITY!

Our community is FREE to join. To participate you must either login or register for an account.

SEARCH FORUMS
FREE NEWSLETTER
By signing up you may also receive reader surveys and occasional special offers. We do not sell, rent or trade our email lists. View our Privacy Policy.